sales@mirrorglabrous.com

+86-21-54419140

Metal Surface Treatment
Complete Solution Provider

Micro-arc Oxidation Equipment for Aluminium Alloy, Titanium Alloy, and Magnesium Alloy


This equipment is used for micro-arc hard oxidation surface treatment for metals such as aluminum alloy, magnesium alloy, titanium alloy. It uses the micro-arc discharge phenomenon to make micro-plasma oxidation reactions on the surface of the anode of the workpiece, and generate high-quality reinforced ceramic films on the surface of the workpiece made of metals such as aluminum, titanium, magnesium and their alloys. The equipment dramatically improves the surface wear resistance, corrosion resistance, insulation resistance, and heat resistance of the workpiece. The process and equipment enable fast film-forming speed, high film hardness, and simple procedures; the metal surface with films has high wear resistance, high insulation, and high corrosion resistance.



The standard process of micro-arc hard anodizing:


Micro-arc Oxidation Equipment for Aluminium Alloy, Titanium Alloy, and Magnesium Alloy



Equipment specifications and performance indicators:

Specifications Unit MIR-MAO-TI MIR-MAO-MG MIR-MAO-AL
Machinable materials   titanium, titanium alloy 镁、镁合金 铝、铝合金
The output voltage V 0~300 0~500 0~750
Equipment power kw 30~450, 50Hz±10%,three-phase five-wire system
Oxide film thickness um 0~100 2~150 40~300
Film hardness Hv 300~1200 300~1200 400~2500
Neutral salt spray test h ≥1000 48~500 ≥500
Wear resistance Increase by 3 to 30 times
提高3~30倍
提高8~50倍
Oxide film color gray, gray black 灰白 灰白、灰黑
Bonding strength with substrate axial tension >60Mpa
shear >25Mpa
轴向拉>70Mpa
剪切>30Mpa
轴向拉伸>70Mpa
剪切>35Mpa
Flexibility average
Working power positive and negative pulse power supply, duty cycle (5 ~ 95%), (100 ~ 2000Hz) adjustable
Auxiliary cathode 316L stainless steel
Control method manual or automatic
Processing quality in accordance with customer demands
Control precision ≤1%
Protection method overcurrent, short circuit, phase loss, overheating protection
Environment condition ambient temperature: 0 ℃ ~ 50 ℃, ambient humidity: ≤80%
Cooling method configured refrigeration unit, refrigeration temperature: 0 ~ 20 ℃

Note: According to the requirements, the positive and negative pulse widths can be adjusted separately, and the number of positive and negative pulses (setting range 0 to 30) can be adjusted in any combination;

Product
MoreNews
10/16 2023

Information on Stain...

5. 摘要 Summary 鉴于大量的影响参数和由此产...

10/07 2023

Information on Stain...

4.3 电化学(阳极)清洗 Electrochemical (anod...

09/25 2023

Information on Stain...

4.2 化学去除方法 Methods of chemical remova ...

09/18 2023

Information on Stain...

3. 清洁和维护 腔室 Cleaning and m...

09/14 2023

上海脉诺金属表面处理...

时间:2023年9月22日 地址:浙江温州温德姆酒...

Contact US
  • Equipment Sales:
    Mr. Wang: +86-15921887786
    Mr. Li: +86-18017268222
    Processing Service:
    Ms. Zhang: 18001952488
    Ms. Long:13386001718

  • Add.: No. 8 Xinshun Road, Zhujing Industrial Park, Zhujing Town, Jinshan, Shanghai, China

  • Email:
    sales@mirrorglabrous.com